component
Anionic surfactant and nonionic surfactant complex
Product performance *)
Molecular weight
It's about 8,000 grams per mole
Available substance content
About 90%
Appearance 20 °C
Fine yellowish powder
pH (DIN 53996), 1% water solution
10-11
biodegradability
Hostapur OSB is easy to biodegrade.
Processing and storage
Hostapur OSB must be stored in a dry place in an airtight container to prevent moisture absorption and caking of powder.
use
Hostapur OSB as an entrainment and a wetting agent, gypsum and lime based on cement mortar and plaster has the following properties:
Hostapur OSB results in faster wetting and drying of mixed solid particles. OSB is fast dissolving Hostapur to develop microfoam in a short time.
Hostapur OSB is capable of rapid air entrainment in mortar and stucco and controllable air content of 20-35%. In establishing Hostapur OSB pores -- cement or cement lime mortar or gypsum board has strong stability.
Hostapur OSB is a product that improves plasticity and workability.
Hostapur OSB is highly efficient and improves mortar performance.
Additive amount
0.005% - 0.025% of the dry component of the building mixture